Die Casting Materials Available At Neway

At Neway, we offer a wide range of die-casting materials, including high-quality aluminum, zinc, and copper alloys. These materials provide excellent strength, durability, and corrosion resistance, making them ideal for various industrial applications and custom parts manufacturing.
Send us your designs and specifications for a free quotation
All uploaded files are secure and confidential

Casting Materials Available At Neway

At Neway, we provide a diverse selection of casting materials, including aluminum alloys, zinc alloys, copper alloys, and premium tool materials. These materials offer outstanding strength, durability, and performance, ensuring high-quality, reliable cast parts for various industries and applications.

Typical Casting Aluminum Alloy Available

We offer a range of high-quality aluminum alloys for die casting, including A356, A360, A380, ADC12 (A383), B390, A413, and anodized aluminum. Each alloy provides unique properties suited for various industries like automotive, aerospace, and electronics.

Aluminum

Aliases

Tensile Strength
(MPa)

Yield Strength
(MPa)

Fatigue Strength
(MPa)

Elongation
(%)

Hardness
(HB)

Density
(g/cm³)

Applications

A380

AlSi9Cu3 (EU), AC7A (Japan)

240-310

155-210

90-120

1-3

90-120

2.68-2.75

Automotive parts, industrial castings, housings

A356

AlSi7Mg (EU)

290-350

230-280

150-180

4-8

120-150

2.68-2.75

Aerospace, high-performance automotive, structural parts

A413

A383 (Japan)

240-310

150-200

85-110

2-4

85-115

2.68-2.75

Precision castings, thin-walled components

A360

AlSi9Cu3 (EU)

250-310

180-230

100-120

3-5

95-120

2.65-2.75

Automotive, industrial components, pressure die casting

AC4C

A360 (US), AlSi9Cu3 (EU)

240-310

170-220

90-120

3-5

95-120

2.65-2.75

Automotive, high-performance die casting

AC7A

A380 (US), AlSi8Cu3 (EU)

230-300

150-200

80-100

2-4

90-115

2.65-2.75

Automotive, industrial, general-purpose die casting

AC8A

A413 (US)

210-280

140-190

75-90

3-5

85-110

2.60-2.75

Automotive, thin-walled parts, precision die casting

AlSi12

AlSi12 (EU)

200-270

150-220

80-100

2-4

85-110

2.60-2.70

Automotive, high-performance, wear-resistant parts

AlZn10Si8Mg

A356 (US)

350-400

270-350

180-220

5-7

150-170

2.60-2.70

Engine components, structural and high-strength parts

Zinc/Zamak Alloys

Aliases

Tensile Strength
(MPa)

Yield Strength
(MPa)

Fatigue Strength
(MPa)

Elongation
(%)

Hardness
(HB)

Density
(g/cm³)

Applications

Zamak 3

ZA-3 (US), ZL3 (EU)

260-310

200-240

100-150

1-3%

80-100

6.60-6.70

General-purpose die casting, automotive parts, hardware

Zamak 5

ZA-5 (US), ZL5 (EU)

270-340

210-250

110-160

2-4%

85-110

6.60-6.70

Electronics, automotive components, decorative parts

Zamak 2

ZA-2 (US), ZL2 (EU)

350-400

250-300

130-180

1-2%

90-120

6.70-6.75

High-strength applications, automotive parts, hardware

Zamak 7

ZA-7 (US), ZL7 (EU)

220-270

180-220

80-120

1-2%

75-95

6.65-6.75

Precision die casting, thin-walled parts

Zamak 8

ZL8 (EU)

240-300

190-230

100-140

2-3%

80-100

6.60-6.70

High-performance applications, automotive, appliance parts

ZA-8

ZL8 (EU)

340-410

250-300

130-180

2-3%

95-120

6.70-6.75

High-strength structural components, automotive parts

Zamak 12

ZL12 (EU)

240-300

190-230

100-140

2-3%

85-100

6.60-6.70

Automotive, machinery, general-purpose parts

Zamak 27

ZL27 (EU)

340-380

250-300

130-180

3-4%

90-120

6.65-6.70

High-performance applications, industrial components

Zinc-Aluminum

ZAMAK 27A

300-380

220-270

120-170

2-3%

90-115

6.60-6.75

Structural parts, industrial and automotive parts

Copper/Brass Alloys

Aliases

Tensile Strength
(MPa)

Yield Strength
(MPa)

Fatigue Strength
(MPa)

Elongation
(%)

Hardness
(HB)

Density
(g/cm³)

Applications

CuZn37

CW510L (EU), C23000 (US)

350-450

220-300

100-150

25-30%

60-90

8.40-8.60

General-purpose brass, plumbing fittings, hardware

CuZn40

CW507L (EU), C24000 (US)

370-460

230-310

110-160

20-30%

80-100

8.40-8.60

Automotive, electrical components, marine hardware

CuZn10

CW508L (EU), C26000 (US)

330-420

210-280

90-130

25-35%

60-90

8.50-8.70

Electrical parts, connectors, architectural hardware

Brass 360

C36000 (US)

520-690

340-420

150-220

30-40%

70-120

8.40-8.60

Precision machining, electrical connectors, fasteners

Brass 380

C38000 (US), CuZn38 (EU)

420-530

270-350

120-180

15-25%

60-90

8.50-8.70

Electrical components, valves, pumps, mechanical parts

Brass 464

C46400 (US)

450-550

300-380

130-200

20-30%

85-110

8.60-8.80

Marine hardware, fittings, pumps, valves

CuNi10Fe1

CW351H (EU)

300-450

210-290

100-160

15-20%

60-90

8.70-8.90

Marine components, valves, pump parts, heavy-duty fittings

CuNi30Fe1

CW352H (EU)

330-480

220-310

110-170

15-20%

70-100

8.70-8.90

Marine applications, chemical and water industry

C17500

Beryllium Copper (US)

690-1100

450-850

250-350

3-5%

160-200

8.35-8.45

High-strength electrical contacts, connectors, springs

C18200

Beryllium Copper (US)

600-1000

400-800

220-320

4-7%

150-200

8.35-8.45

Aerospace, electrical contacts, high-performance springs

Let's Start A New Project Today

Frequently Asked Questions

Explore Related Blogs

Explore Related Resources

Neway Precision Works Ltd.
No. 3, Lefushan Industrial West Road
Fenggang, Dongguan, Guangdong
China (ZIP 523000)
Copyright © 2025 Diecast Precision Works Ltd.All Rights Reserved.